Figure 1.

Scanning electron micrographs of a zirconia disk (left) showing occasionally pores on the smooth surface and a titanium disk (right) with rough surface and frequent pores and grooves of different size (2 kV, magnification 500-fold).

Depprich et al. Head & Face Medicine 2008 4:29   doi:10.1186/1746-160X-4-29